The die-casting mold must be fully tempered, usually three times.
The first tempering temperature is selected within the secondary hardening temperature range;
The second tempering temperature should be selected so that the mold reaches the required hardness;
The third tempering should be 10℃-20℃ lower than the second time.
After tempering, oil cooling or air cooling is used, and the tempering time is not less than 2 hours.