1. Poor corrosion resistance
When the impurity elements lead, cadmium, and tin in the alloy composition exceed the standards, the castings will age and deform, manifesting as volume expansion, significant decrease in mechanical properties, especially plasticity, and even rupture over time. The solubility of lead, tin, and cadmium in zinc alloys is very small, so they are concentrated at the grain boundaries and become the cathode. The aluminum-rich solid solution becomes the anode, which promotes intergranular electrochemical corrosion in the presence of water vapor (electrolyte). Die castings age due to intergranular corrosion.
2. Time effect
The structure of zinc alloy is mainly composed of zinc-rich solid solution containing Al and Cu and Al-rich solid solution containing Zn. Their solubility decreases with the decrease of temperature. However, due to the solidification speed of die castings, the solubility of the solid solution is saturated at room temperature. After time, this supersaturation phenomenon will gradually be relieved, causing the shape and size of the casting to change slightly.
3. Not suitable for use at high or low temperatures
Die castings should not be used in high and low temperature (below 0°C) working environments. Zinc alloy has good mechanical properties at room temperature. However, the tensile strength at high temperatures and the impact properties at low temperatures decrease significantly.
Factors that can reduce thermal stress, improve the high-temperature strength and toughness of the sand core, and accelerate the solidification of molten iron will reduce the occurrence of veins.
Practice has proven that the tendency of resin sand to produce vein defects is in the following order: cold core box resin sand ~ PEPSET resin sand ~ coated sand ~ furan resin sand ~ alkaline phenolic resin sand